hastelloy C-276

본문 바로가기


Home > Product > hastelloy C-276
Product
hastelloy C-276
Posting date : Oct 18, 2012
Membership
Free Member Scince Oct 18, 2012
Keyword :
Category
Contact
          0 likes     
Product Detail
Company Info
 
Quick Detail
Place of Origin
HS-CODE
75-
Package & Delivery Lead Time
Detailed Description
Hastelloy C-276(UNS N10276)tungsten-nickel-chromium-molybdenum alloy Features and applications overview: The alloy has excellent corrosion to the majority of corrosive media in the oxidation and reduction state. It has excellent resistance to pitting corrosion, crevice corrosion, and stress corrosion cracking. The alloy is suitable for containing various oxidizing and reducing media industrial chemical processes. High molybdenum and chromium content of the alloy can be resistant to chloride ion erosion, and tungsten element also further improves its corrosion resistance. Hastelloy C-276 is one of the only several materials resistant to the corrosion of wet chlorine gas, hydrochloride and chlorine dioxide solution. The alloy has significant corrosion resistance to the high concentration of chloride salts, such as iron chloride and copper chloride. Hastelloy C-276's similar grades: W.Nr.2.4819 NiMo16Cr15W (Germany) NC17D (France) Chemical composition, %: Nickel........................................balance Chromium..................................15.0-16.5 Iron.............................................4.0-7.0 Molybdenum..............................15.0-17.0 Cobalt.........................................2.5 max Carbon........................................0.01 max Manganese..................................1.0 max Silicon.........................................0.08 max Sulfur...........................................0.001 max Phosphorus...................................0.015 max Tungsten........................................3.0-4.5 Vanadium.......................................0.1-0.3 Physical properties: Density, g/cm3 ....................................................8.9 Melting Range, °C...............................................1325-1370 Thermal conductivity, λ/(W/m•°C), at 100°C ......10.2 Specific heat, J/kg•°C.............................................407 Elastic modulus, GPa............................................208 Shear modulus, GPa...........................................79 Electrical resistivity, μΩ•m..................................1.25 Coefficient of linear expansion, a/10-6°C-1, at 20-100°C........11.7 Mechanical properties:(the minimum value detected at room temperature) Tensile strength, σb/MPa.....................................758 Yield strength,σp0.2/MPa...............................363 Elongation,σ5 /%...................................................................62 The way of heat treatment is solution treatment Available products and specifications: Bar: ASTM B574, ASME SB574 Forging: ASTM B564, ASME SB564 Plate/Strip: ASTM B575, ASME SB575 Pipe: ASTM B622, ASTM B619, ASTM B626, ASME SB622, ASME SB619, ASME626 The metallurgical structure of Hastelloy C-276: Hastelloy C-276 is of the face-centered cubic lattice structure. The process performance and requirements of Hastelloy C-276: 1, The content of sulfur in fuel should be kept as low as possible. The sulfur content of the gas should be less than 0.1%, and in heavy oil should be less than 0.5%. 2, The thermal processing temperature range of the alloy is 1200°C-950°C. The cooling method is water-cooling or other rapid cooling. 3, All conventional welding processes is suitable to apply, such as tungsten electrode inert gas welding, plasma arc welding, handmade sub-arc welding, and metal inert gas shielded arc welding.

ECROBOT CO., Ltd, Business Registration Number : 220-88-71747, CEO J.W.Park, TEL : +82-2-552-7676, E-mail : E-mail : Contact us
Address : (Hwanghwa B/D 11F, Yeoksam-dong)320, Gangnam-daero, Gangnam-gu, Seoul, South Korea
About Us Privacy Policy Terms of use Copyright © 2000-2024 ECROBOT.COM. All rights reserved.
Top