Chemical Composition% |
|||||||
Si |
Mg |
Ca |
Re |
Ba |
La |
Fe |
|
BN-126 |
38-44 |
6-7.5 |
1.0-3.0 |
1.8-2.5 |
- |
|
balance |
BN-127 |
38-44 |
6.3-7.5 |
2.0-3.5 |
2.5-4.0 |
1.2-2.0 |
|
balance |
BN-137 |
38-44 |
6.3-7.5 |
1.0-3.0 |
2.5-4.0 |
- |
|
balance |
BN-138 |
38-44 |
7.0-9.0 |
2.0-3.0 |
2.0-4.0 |
- |
|
balance |
BN-158 |
38-44 |
7.0-9.0 |
2.0-3.0 |
4.0-6.0 |
- |
|
balance |
BN-101 |
44-48 |
5.6-6.5 |
0.8-1.2 |
- |
<2.0 |
proper |
balance |
BN-104 |
44-48 |
5.5-6.5 |
1.0-1.5 |
0.4-0.6 |
proper |
|
balance |
1.Ferro Silicon Magnesium Alloy is shaped in gray lump with metal luster. It is solid and brittle so that it is easy to be smashed.
2.With stable reaction, the absorption rate of Mg. will be increased which is helpful for getting high-quality casting products.
3.High mechanical strength and strong deoxygenation and desulfuration effects.
Sarah Ye
Jiangsu Benai Alloys Co.,Ltd.
Add.: South Area,Industrial Convergence Zone,Benniu Town,
Xinbei District,Changzhou,Jiangsu,China
E-mail:wjh@benai.cn
Mobile: +86-15861159194
WhatsApp/Wechat: +86-15861159194
Website: www.benai.cn