Appearance | White to off-white powder |
---|---|
Particle size | 80,100,120mesh |
Methoxyl content(%) | 19-25 |
Hydroxypropyloxy content(%) | 4.0-12.0 |
Gelation temperature(℃) | 60-90 |
Moisture (%) | ≤5.0 |
PH value | 5.0-7.5 |
Residue on ignition | ≤1.0 |
Types | Viscosity (Brookfield, mPa.s, 2%) | Viscosity (NDJ-1, mPa.s, 2%) |
---|---|---|
HPMC 75MP400 | 320-480 | 320-480 |
HPMC 75MP10M | 10000 | 10000 |
HPMC 75MP40M | 20000 | 40000 |
HPMC 75MP75M | 35000 | 75000 |
HPMC 75MP100M | 40000-55000 | 80000-120000 |
HPMC 75MP150M | 55000-65000 | 120000-180000 |
HPMC 75MP200M | Min65000 | 160000-240000 |
HPMC 75MP4000S | 4000 | 4000 |
HPMC 75MP60MS | 24000-36000 | 48000-72000 |
HPMC 75MP100MS | 40000-55000 | 80000-120000 |
HPMC 75MP150MS | 55000-65000 | 120000-180000 |
HPMC MP200MS | Min65000 | 160000-240000 |
Remarks: S means surface treated
Tile Adhesive
1 Good water retention: it can prolonged opening time , to make tiling more efficient
2 Improved adhesion and sliding resistance especially for heavy tiles
3 Better work-ability: lubricity and plasticity of plaster is ensured, mortar can be applied easier and quicker
Cement Based Plaster
1 Easy dry mix formulation due to cold water solubility: lump formation can be easily avoided, ideal for heavy tiles.
2 Good water retention: prevention of fluid loss to the substrates, the appropriate water content is kept in mixture which guarantees longer concreting time
3 Increased water demand: increased open time, expanded spry area and more economical formulation
4 Easier spreading and improved sagging resistance due to improved consistency
Exterior Heat Insulation System ( EIFS )
1 Improved adhesion
2 Good wetting ability for EPS board and substrate
3 Reduced air entrainment and water uptake.
Self-leveling
1 Protection from water exudation and material sedimentation
2 No effect on slurry fluidity with low viscosity HPMC, while its water retention characteristics improve the finish performance on the surface.
Crack Filler
1 Better workability: proper thickness and plasticity
2 Water retention ensures prolonged work time
3 Sag resistance: improved mortar bonding ability
Gypsum Based Plaster
1 Water retention: maximized water content in slurry ensures complete gypsum concretion.
2 Anti-sagging: when spreading a thicker coat corrugation can be avoided ( careful when air is entrained )
3 Increased mortar yield: depending on the weight of the dry mixture and appropriate formulation HPMC can increase the mortar
Ceramic Extrusion
1 Excellent workability for ceramic molding due to lubricity and plasticity
2 Compact texture and smooth surface of ceramic product due to negligible ash content