Ceramic Fiber Module
|
HR1050
|
HR1260ST
|
HR1260HP
|
HR1350
HA
|
HR1430Zr
|
HR1600
PMF
|
|
Classification Temperature
(℃)
|
1050
|
1260
|
1260
|
1350
|
1430
|
1600
|
|
192kg/m3/at( )℃/24h
Linear Shrinkage Rate(%)
|
≤2.0
850℃
|
≤2.0
1000℃
|
≤2.2
1050℃
|
≤2.2
1100℃
|
≤2.5
1200℃
|
≤1.5
1450℃
|
|
Density(KG/M3)
|
172-240
|
172-240
|
172-240
|
172-240
|
172-240
|
172-240
|
|
Thermal Conductivity Rate(W/m.k)
|
400℃
|
0.08
|
0.08
|
0.08
|
0.08
|
0.08
|
-
|
600℃
|
0.15
|
0.15
|
0.15
|
0.12
|
0.12
|
0.12
|
|
800℃
|
0.22
|
0.20
|
0.19
|
0.18
|
0.16
|
0.15
|
|
1000℃
|
-
|
-
|
0.22
|
0.12
|
0.19
|
0.18
|
|
Chemical Composition(%)
|
Al2O3
|
42-44
|
45-46
|
47-49
|
52-55
|
38-44
|
72-75
|
Al2O3+SiO2
|
≥99.0
|
≥99.0
|
≥99.0
|
≥99.0
|
≥99.0
|
≥99.0
|
|
ZrO3
|
-
|
-
|
-
|
-
|
15-17
|
-
|
|
Other
|
≤1.0
|
≤1.0
|
≤1.0
|
≤1.0
|
≤1.0
|
≤1.0
|