SPECIFICATION(BUILDING&CERAMICS)
TYPE/SPECIFICATION
|
VISCOSITY
(4%SOLUTION, 25°C)mpa.s(B)
|
DEGREE OF SUBSTI-TUTE(D.S)
|
pH VALUE
|
CHLORIDE
(NaCL%)
|
MOISTURE
(%)
|
HEAVY METALS
(pb%)
|
ARSENIC
(%)
|
IRON
(%)
|
TCH6-1
|
900-1200
|
≥0.65
|
6.0-8.5
|
≤20
|
≤10.0
|
-
|
-
|
-
|
TCH6-2
|
900-1200
|
≥0.65
|
6.0-8.5
|
≤15
|
≤10.0
|
-
|
-
|
-
|
TCM6
|
400-600
|
≥0.65
|
6.0-8.5
|
≤20
|
≤10.0
|
-
|
-
|
-
|
TCH9-1
|
900-1200
|
≥0.92
|
6.5-8.0
|
≤3
|
≤10.0
|
≤0.002
|
≤0.0005
|
≤0.03
|
TCH9-2
|
1200-1500
|
≥0.92
|
6.5-8.0
|
≤3
|
≤10.0
|
≤0.002
|
≤0.0005
|
≤0.03
|
TCL9
|
20-50
|
≥0.92
|
6.5-8.0
|
≤3
|
≤10.0
|
≤0.002
|
≤0.0005
|
≤0.03
|
TCM9
|
400-600
|
≥0.92
|
6.5-8.0
|
≤3
|
≤10.0
|
≤0.002
|
≤0.0005
|
≤0.03
|
CMC is applied in building coating industry:
CMC is applied in hydrolactoprence urushi, because it has rheological nature. It can get a certain flowing performance, under the action of brush and tumbling box shear force.
At the same time, it can control viscosity and floating.
CMC occupy 1-3 percent in hydro coating.
CMC is applied in ceramics industry:
CMC can be applied as semi-finished viscosity in ceramics industry, for it can increase plasticity performance.
CMC can be used as flowing control matter in ceramics glost substitute, which has the performance of retain glost substitute, to prevent it from getting to tear cicatrices before cooking finish.
At the same time, it can be burned out.
Packing:
Our product is packed in double layer bags with polyethylene film bag enclosed
in coated plastic woven bag. The net weight is 25kg/bag. The products can also
be packed as you request.
Delivery:
We will deliver the products within 10 to 15 working days after the deposit has
been confirmed. We usually choose FOB as delivery method.